av在线不卡擦哦_99热精国产这里只有精品_亚洲国产另类无码_亚洲福利在线一区少妇

Product features

The melting process of the material is optimized, so as to increase the extrusion yield and realize the extrusion of the material melt at a lower temperature.

Good homogenization of the material is achieved by the specific shear action in the isolation gap.

The melt plasticization process is controlled, meaning that only particles smaller than the isolation gap can enter the melt channel.


Extrusion screw - Pipe screw

Material: 38 crmoala

Process: nitriding and bimetallic

Nitriding depth: 0.5mm-0.7mm

Bimetallic screw: alloy layer hardness HRC>60

Nitriding layer hardness: HV960-1100

Alloy layer depth: 2~2.5

Screw straightness: 0.015mm

Chrome plated screw: Chromium layer thickness: 0.03-0.06mm

Surface finish: 0.04Ra/um~0.08Ra/um

Nitride brittleness: less than grade 2

Aspect ratio: 1: (33~42)